| Kwaliteit | Ni% | CR% | FE% | C% | MN% | S% | SI% | Cu% | Al% | TI% |
| Incoloy 800 | 30.0-35.0 | 19.0-23.0 | Min. 39.5 | Max. 0.10 | Max. 1.50 | Max. 0.015 | Max. 1.0 | Max. 0.75 | 0.15-0.60 | 0.15-0.60 |
| Kwaliteit | Ni% | CR% | FE% | C% | MN% | SI% | Cu% | S% | AL% | TI% | Al+Ti% |
| Incoloy 800H | 30.5-35.0 | 19.0-23.0 | Bal. | 0.05-0.10 | Max. 1.5 | Max. 1.0 | Max. 0.75 | Max. 0.015 | 0.15-0.60 | 0.15-0.60 | 0.30-1.20 |
| Incoloy 800HT | 30.0-35.0 | 19.0-23.0 | Bal. | 0.06-0.10 | Max. 1.5 | Max. 1.0 | Max. 0.75 | Max. 0.015 | 0.25-0.60 | 0.25-0.60 | 0.85-1.20 |
| Kwaliteit | UNS | Werkstoff Nr. |
| Incoloy 800 | N08800 | 1.4876 |
| Kwaliteit | UNS | Werkstoff Nr. |
| Incoloy 800H | N08810 | 1.4958 |
| Incoloy 800HT | N08811 | 1.4959 |
| Kwaliteit | Dichtheid | Smeltpunt |
| Incoloy 800 | 8.0 g/cm3 | 1350 °C-1400 °C. |
| Kwaliteit | Dichtheid | Smeltpunt |
| Incoloy 800H/800HT | 8.0 g/cm3 | 1370 °C-1400 °C. |
| Kwaliteit | Treksterkte | Opbrengststerkte | Verlenging |
| Incoloy 800 | 520 N/mm² | 205 N/mm² | 30% |
| Legering | Treksterkte | Opbrengststerkte | Verlenging |
| Incoloy 800H/800HT | 450 N/mm² | 170 N/mm² | 35% |